ARTICLE
👁 1
⏱ ~1 min read
2205 · welding · duplex
2205 Duplex Steel Welding: Heat Input and Ferrite Control
Phase balance, heat input range, and common defects in duplex steel welding.
Duplex welding requires controlled heat input (typically 0.5-2.5 kJ/mm), balanced filler (e.g. 2209), and avoiding excessive ferrite or sigma phase. Purge and interpass temperature matter.
Compiled by SteelWe editors and industry experts. For industry exchange only; not trading or investment advice. Cite the source when quoting.