拉丝机砂带目数怎么选

孙孙表面·11/3/2026, 1:59:13 AM👁 102

304 拉丝板,客户要 No.4 效果。砂带从粗到细怎么配?

#拉丝#砂带#表面
Plain text; no ads

Replies (1)

孙
孙表面11/7/2026

No.4 一般从 60-80 目粗磨到 120-150 目定型,最后一道决定纹路细腻度,别跳目数。